Sprayon S00744 & S00745 Welding Defect Detector- Penetrant & Developer, Two-Part Q. A. System WL 744 & WL 745 - S00744 Penetrant & S00745 Developer

Sprayon Welding Defect Detector- Penetrant & Developer

Sprayon S00744 & S00745 Welding Defect Detector- Penetrant & Developer, Two-Part Q. A. System WL 744 & WL 745 - S00744 Penetrant & S00745 Developer


PLEASE READ - Sprayon $425 Minimum Order Policy Before Proceeding to Checkout (Click Here)


Sprayon Logo



Please Call 931-651-1044 for Large Volume Custom Quote!


In addition to  FREE Freight, ALL Sprayon orders exceeding $1,500 receive 10% off at Checkout!

Free Shipping on $149 or More!




Free Shipping on Orders of $149+
Use Coupon Code FREESHIP at Checkout


**PLEASE READ the Sprayon Minimum Order Policy & Check the Box Below.  The Box MUST BE CHECKED in Order to Add an Item to the Cart**


Be the first to review this product

2-Part System
$179.63

* Required Fields

Sprayon S00744 & S00745 Welding Defect Detector- Penetrant & Developer, Two-Part Q. A. System
Item: S00744 & S00745 / 5S - WL 744 & WL 745

Sprayon® WL™ 744 and WL™ 745 Welding Defect Detector is a two-part quality assurance system that detects and locates cracks and defects in metals and non-porous, non-metal parts. You can be confident that Sprayon's Welding Defect Detector crack detecting system will detect and clearly mark even the finest faults in welds, casts and other non-porous materials before they cause product failure or costly breakdowns. Welding Defect Detector is ideal for short run applications where production testing sites are not available, or for spot-testing large parts, welds, assemblies and more. It is specially suited for the precise, very fine inspections required in the auto, construction, manufacturing, nuclear power, petroleum, foundry and railroad industries.

Step 1
On a Pre-Cleaned surface (We recommend Sprayon S00848 Flash Free Safety Solvent / Degreaser), spray the S00744 Penetrant and let it seep into any cracks

Step 2
Then wipe the surface and spray the S00745 Developer.  Faults, cracks or pores will be revealed in RED

Uses:  Turbine blades, molds, structural beams, pipes, other metal and nonporous, nonmetal parts

  • Two-part quality assurance system
  • Detects and locates cracks and defects in metals and non-porous, non-metal parts
  • Meets or exceeds performance requirements to MIL-L-25135
  • Meets or exceeds performance requirements for NAVSHIPS 250-1500 MIL STD 271-D


WL 744 Performance Properties-

Appearance: TRANSLUCENT RED
Propellant: HYDROCARBON BLEND
Specific Gravity: 0.73
Percent VOC: 98.7
VOC Compliant (CA and OTC States): Y
Flash Point: <0
Flammable: Y
HMIS: 2,4,0
Fill Weight: 9
Size UOM: oz
Can Type: Aerosol

 
















WL 745 Performance Properties-

Appearance: POWDER WHITE
Propellant: HYDROCARBON BLEND
Specific Gravity: 0.64
Percent VOC: 95
VOC Compliant (CA and OTC States): Y
Flash Point: <0
Flammable: Y
HMIS: 2,4,0
Fill Weight: 7
Size UOM: oz
Can Type: Aerosol


Tech Specs
Meets or exceeds performance requirements to MIL-L-25135
Meets or exceeds performance requirements for NAVSHIPS 250-1500 MIL STD 271-D
Uses: Turbine blades, molds, structural beams, pipes, other metal and nonporous, nonmetal parts.